Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Zone 2 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |