Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1451L Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1563 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1579D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1580D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1646-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1652B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1870A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2215 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2315C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2318 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1205A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1366C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2434G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Consumer Applications; Gaskets; Medical/Healthcare Applications; Membranes; Packaging; Safety Equipment; Sporting Goods; Tape; Tubing Forms: Pellets Processing Method: Fi.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2455 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2455S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2560B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2664B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2870UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2604B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2691A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Zone 2 | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2875M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |