Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 - 250 °C | 437 - 482 °F | Middle |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 2 | 225 - 250 °C | 437 - 482 °F | Middle |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |