Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | Blow Molding |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | |
Lehmann & Voss LUVOCOM® TPE-0900 VP Thermoplastic elastomer, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | |
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | |
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect†on the f.. |
|||
Zone 2 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 2 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | Injection |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | Injection |
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MF0044 PP, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam MF0044 is a Halogen Free Flame Retardant, Glass Fiber Reinforced, PP Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |