Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 170 °C | 338 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 2 | 170 °C | 338 °F | |
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 2 | 170 °C | 338 °F | |
Termopol Termoton® V6GA3075A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Zone 2 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 170 - 185 °C | 338 - 365 °F | Extrusion Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Zone 2 | 170 - 180 °C | 338 - 356 °F | Extrusion Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 2 | 170 °C | 338 °F | |
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Zone 2 | 170 - 180 °C | 338 - 356 °F | |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 2 | 170 - 180 °C | 338 - 356 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Borcell™ HE1346 High Density Polyethylene Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent.
Applications Borcell™ HE.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Visico™/Visico™ LE4421/LE4438 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4421 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Zone 2 | 170 °C | 338 °F | Extrusion |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Zone 2 | 170 °C | 338 °F | Extrusion |
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance re.. |
|||
Zone 2 | 170 - 182 °C | 338 - 360 °F | Extrusion |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442.. |
|||
Zone 2 | 170 °C | 338 °F | |
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas.. |
|||
Zone 2 | 170 °C | 338 °F | |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |