Polymer Property : Zone 2 = 149 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 149 °C
300 °F
LyondellBasell Aquathene® CM04482 Catalyst Masterbatch
ApplicationsAQUATHENE CM 04482 is a catalyst masterbatch designed for use with AQUATHENE AQ 120-000 ethylene vinylsilane copolymer. When CM 04482 is added at 5 wt% to AQ 120-000, the resulting mate..
Zone 2 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed ..
Zone 2 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® NA951080 Low Density Polyethylene
ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium..
Zone 2 149 °C
300 °F
LyondellBasell Aquathene® CM92949B Black Masterbatch
ApplicationsAQUATHENE CM 92949 is a black masterbatch designed for use with AQUATHENE AQ 120-00 ethylene vinylsilane copolymer for producing low voltage, power insulation. When CM 92949 is added at..
Zone 2 149 - 193 °C
300 - 379 °F
Styrolution PS-168M Polystyrene
Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M i..