| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7652 Polyamide 46, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at e..
|
|||
| Zone 1 | 285 - 315 °C | 545 - 599 °F | |
|
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te..
|
|||