| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 190 - 210 °C | 374 - 410 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
| Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
| LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
| Zone 1 | 190 °C | 374 °F | |
| Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
| Zone 1 | 190 °C | 374 °F | |
| SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
| Zone 1 | 190 °C | 374 °F | Injection Molding |
| UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 - 220 °C | 374 - 428 °F | |
| Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
| Zone 1 | 190 - 220 °C | 374 - 428 °F | |
| Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
| Zone 1 | 190 - 200 °C | 374 - 392 °F | Injection |
| Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Fuel C for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 °C | 374 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Zone 1 | 190 - 230 °C | 374 - 446 °F | |
| Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
| Zone 1 | 190 °C | 374 °F | Extrusion |
| Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Zone 1 | 190 °C | 374 °F | Extrusion |
| Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
| Zone 1 | 190 - 200 °C | 374 - 392 °F | |
| Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio.. |
|||