Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7719/BN PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Isotropic shrinkage characteristics.Emergency running property.Information provided by Leh.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8059 PEEK, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/RD7405 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0950/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8127-1 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8135/OR PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |