Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL 83-F943D22-NT Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1035-70 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1081B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1524E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1949A-55NT Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2478H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2565F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3954-50 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-81-D920-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-89-P834-B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-94-T0586C-113 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 204 °C | 330 - 400 °F | |
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Zone 1 | 166 - 204 °C | 330 - 400 °F | |
Teknor Apex Uniprene® UN-2640S Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Zone 1 | 166 - 204 °C | 330 - 400 °F | |
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3954-45 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-91-T3056S-90 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 °C | 330 °F | |
Axiall 3803 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |