Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® V6GA3075A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis Borcell™ HE4873 High Density Polyethylene Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |