Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 260 - 270 °C | 500 - 518 °F | hopper |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide A28 PA66, Injection Molding Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide R1000IX2 PA66, Impact Modified, Injection Molded Staramide R1000IX2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as Star X 1010)Information provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |