Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 240 °C | 464 °F | Die |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8282 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam BFR460B PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX06020 PA6, Flame Retardant, Injection Molded Starflam PX06020 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX07037 PA6, Flame Retardant, Injection Molded Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)Information provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 °C | 464 °F | Feeding zone |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |