Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol.. |
|||
Zone 1 | 130 °C | 266 °F | |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Fainplast Compounds HAX HF 200 Halogen Free PVC HAX HF 200 is a thermoplastic flame retardant compound, and halogen free on polyolefinic basis. It can be used for the production of energy, signal and control cables |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 1 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified
(discontinued **) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |