| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Die Temperature | 230 °C | 446 °F | Zone 2 |
| Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
| Die Temperature | 230 °C | 446 °F | Zone 4 |
| Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
| Die Temperature | 230 °C | 446 °F | Zone 4 |
| Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
| Die Temperature | 230 °C | 446 °F | Zone 2 |
| Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
| Die Temperature | 230 °C | 446 °F | Zone 4 |
| Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
| Die Temperature | 230 °C | 446 °F | Zone 4 |
| Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
| Die Temperature | 230 - 240 °C | 446 - 464 °F | Average value: 235 °C Grade Count:3 |
| Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
| Die Temperature | 230 - 250 °C | 446 - 482 °F | Extrusion |
| Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
| Die Temperature | 230 - 240 °C | 446 - 464 °F | |
| Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen.. |
|||
| Die Temperature | 230 - 240 °C | 446 - 464 °F | |
| Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
| Die Temperature | 230 °C | 446 °F | Extrusion |
| Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
| Die Temperature | 230 - 245 °C | 446 - 473 °F | |
| BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
| Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
| UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||