Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 182 - 216 °C | 360 - 421 °F | |
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE) Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl.. |
|||
Die Temperature | 182 - 216 °C | 360 - 421 °F | |
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE) Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci.. |
|||
Die Temperature | 175 - 216 °C | 347 - 421 °F | Average value: 194 °C Grade Count:46 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Die Temperature | 177 - 216 °C | 351 - 421 °F | Extrusion |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |