Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE) Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer.. |
|||
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |
|||
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |
|||
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |
|||
Die Temperature | 171 - 199 °C | 340 - 390 °F | |
PolyOne Versaflex™ HC MT226 Thermoplastic Elastomer (TPE) Versaflex™ HC MT226 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT226 has been specially formulated to be free of any plasticizers . .. |
|||
Die Temperature | 177 - 199 °C | 350 - 390 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |