Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
ExxonMobil Dytron™ XK7300-92 Thermoplastic Elastomer
(discontinued **) A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is flexible and halogen-free, and is intended mainly for extrusion of ca.. |
|||
Die Temperature | 160 - 190 °C | 320 - 374 °F | Extrusion Blow Molding |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Die Temperature | 185 - 190 °C | 365 - 374 °F | |
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications Bormed HD850MO is a medium melt flow rate polypropylene homo polymer using the Borealis Nucleation Technology (BNT). This provides a polypropylene with excellent dimensional stability and its high c.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis Borstar® BB2581 HDPE for Blow Molding Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Die Temperature | 150 - 190 °C | 302 - 374 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 185 - 190 °C | 365 - 374 °F | |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |