Polymer Property : Die Temperature = 365 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 175 - 185 °C
347 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Die Temperature 175 - 185 °C
347 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
Die Temperature 174 - 185 °C
345 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance..
Die Temperature 175 - 185 °C
347 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera..
Die Temperature 174 - 185 °C
345 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
Die Temperature 175 - 185 °C
347 - 365 °F
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance..
Die Temperature 141 - 185 °C
285 - 365 °F
Average value: 174 °C Grade Count:10
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..