Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 204 °C | 399 °F | Zone 1, 6, Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Die Temperature | 204 °C | 399 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Die Temperature | 204 °C | 399 °F | Zone 1, Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Die Temperature | 204 °C | 399 °F | Zone 2, Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Die Temperature | 204 °C | 399 °F | |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Die Temperature | 204 - 218 °C | 399 - 424 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Die Temperature | 204 °C | 399 °F | Zone 1, Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |
|||
Die Temperature | 204 °C | 399 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |