Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 190 - 195 °C | 374 - 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |
|||
Die Temperature | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Die Temperature | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Die Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Die Temperature | 175 - 195 °C | 347 - 383 °F | |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |