Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ.. |
|||
Die Temperature | 174 - 185 °C | 345 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance.. |
|||
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera.. |
|||
Die Temperature | 174 - 185 °C | 345 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance.. |
|||
Die Temperature | 141 - 185 °C | 285 - 365 °F | Average value: 174 °C Grade Count:10 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |