Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 240 °C | 464 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 240 °C | 464 °F | Cast Film |
Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati.. |
|||
Die Temperature | 240 °C | 464 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati.. |
|||
Die Temperature | 240 °C | 464 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |
|||
Die Temperature | 240 °C | 464 °F | |
Solvay TECHNYL® C 502XT PA6, DRY Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, shee.. |