Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Average value: 238 °C Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Die Temperature | 220 °C | 428 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Die Temperature | 220 °C | 428 °F | |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Die Temperature | 220 - 230 °C | 428 - 446 °F | 6 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Die Temperature | 220 °C | 428 °F | |
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 220 °C | 428 °F | Blow Film |
DuPont Appeel® LSR11D542 Lidding Sealant Resin Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Die Temperature | 220 °C | 428 °F | Extrusion |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Average value: 230 °C Grade Count:3 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |