Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 208 °C | 406 °F | Extrusion |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Die Temperature | 208 °C | 406 °F | Extrusion |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |