Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP 1079E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1301A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1479F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1580B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1709A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1776A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1782 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1956A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2100 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2228C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2260-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2322UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1366A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-1855PV2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2581A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2760 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2860M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2870UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 °C | 390 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2850M-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Die Temperature | 199 - 249 °C | 390 - 480 °F | |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |