Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 191 - 210 °C | 375 - 410 °F | |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Die Temperature | >= 191 °C | >= 375 °F | |
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas.. |
|||
Die Temperature | 191 °C | 375 °F | |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Die Temperature | 191 °C | 376 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi.. |
|||
Die Temperature | 191 °C | 376 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Die Temperature | 191 °C | 376 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Die Temperature | 191 - 224 °C | 375 - 435 °F | Extrusion |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |