Processing Properties Metric English Comments
Die Temperature 152 - 157 °C
305 - 315 °F
LyondellBasell Petrothene® YR19548 Polyolefin Compound
ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance ..