Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | 5 |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | 5 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |