Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Adapter Temperature | 327 - 371 °C | 621 - 700 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |