Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion Coating |
DuPont Appeel® LSR20D752 Lidding Sealant Resin Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Adapter Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |