Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Alathon® M5370WC High Density Polyethylene ApplicationsALATHON M 5370WC is a natural, high density, polyethylene copolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cab.. |
|||
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® KR92717 High Density Polyethylene ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun.. |
|||
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® LR590001 High Density Polyethylene ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e.. |
|||
Adapter Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® LR590005 High Density Polyethylene ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains .. |
|||
Adapter Temperature | 246 - 266 °C | 475 - 510 °F | |
Entec Hylex® P1302B Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |