Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 204 °C | 399 °F | 5, Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Adapter Temperature | 204 °C | 399 °F | 5, Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Adapter Temperature | 204 - 218 °C | 399 - 424 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Adapter Temperature | 204 - 216 °C | 399 - 421 °F | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Adapter Temperature | 204 °C | 399 °F | Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |