Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Feed Temperature = 230 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature <= 110 °C
<= 230 °F
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Feed Temperature <= 110 °C
<= 230 °F
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture..