Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Feed Temperature | 260 - 275 °C | 500 - 527 °F | |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Feed Temperature | 260 - 275 °C | 500 - 527 °F | |
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay Technyl® A20V25 25% Glass Filled, V-0 Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 208F PA66, DRY Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY Description: Polyamid 66, reinforced with 38% of glass fiber and mineral filler, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2412GM05-D is used in all sectors o.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |
|||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, DRY Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |