Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 245 - 260 °C | 473 - 500 °F | |
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di.. |
|||
Feed Temperature | 240 - 260 °C | 464 - 500 °F | |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Feed Temperature | 240 - 260 °C | 464 - 500 °F | |
Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 0 Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ?.. |
|||
Feed Temperature | 240 - 260 °C | 464 - 500 °F | |
Solvay TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY Description: Polyamide 6 reinforced with 30% of glass fibers, heat stabilized, with high viscosity and high toughness, for extrusion.Available in: North America Product Applications: This product is.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |