Polymer Property : Feed Temperature = 129 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 129 - 135 °C
265 - 275 °F
LyondellBasell Petrothene® YR19548 Polyolefin Compound
ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance ..