Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | <= 110 °C | <= 230 °F | |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Feed Temperature | <= 110 °C | <= 230 °F | |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |