Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 35 - 45 sec | 35 - 45 sec | |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Cycle Time - Injection | 35 - 45 sec | 35 - 45 sec | |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M104N MPPO Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M105 MPPO Resin Flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M105N MPPO Resin High flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M106 MPPO Resin Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M104 MPPO Resin Flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Cycle Time - Injection | 35 sec | 35 sec | |
Beijing Chemical Industry KAIFA® M106N MPPO Resin High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |