Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 1.00 - 2.50 sec | 1.00 - 2.50 sec | Average value: 1.75 sec Grade Count:6 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |