Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Cycle Time - Injection | 0.50 - 2.0 sec | 0.50 - 2.0 sec | boost |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |