Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 7200 - 86400 sec |
250 - 260 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Drying Temperature | 121 - 127 °C @Time 14400 - 86400 sec |
250 - 260 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |