Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 60.0 °C @Time 1800 sec |
140 °F @Time 0.500 hour |
|
Gwent Electronic Materials C2000215D4 Silver / Silver Chloride Paste C2000215D4 has a ratio of Silver to Silver Chloride of 50/50. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |