Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 0.750 - 60.0 min | 0.750 - 60.0 min | Average value: 10.1 min Grade Count:28 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Pot Life | 40.0 - 60.0 min @Temperature 23.0 °C |
40.0 - 60.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 40.0 - 60.0 min @Temperature 23.0 °C |
40.0 - 60.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |