Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® UR3001HP Black Urethane Encapsulant Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Time before parts must be mated |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | |
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | 100 gm mass |
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | 100 gram batch |
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or .. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | 100 gram mass |
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room .. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | |
Loctite® 3951 Gap filling, flexible Urethane Adhesive Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap.. |
|||
Pot Life | 15 - 20 min @Temperature 24.0 °C |
15 - 20 min @Temperature 75.2 °F |
4 oz. mass |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Pot Life | 16 - 20 min @Temperature 24.0 °C |
16 - 20 min @Temperature 75.2 °F |
|
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Pot Life | 16 - 20 min @Temperature 24.0 °C |
16 - 20 min @Temperature 75.2 °F |
work life |
BCC Products BC 8860 Polyurethane Elastomer BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Pot Life | 18 - 20 min @Temperature 24.0 °C |
18 - 20 min @Temperature 75.2 °F |
|
BCC Products BC 8870 Polyurethane Elastomer BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |