Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 9.00 - 180 min | 9.00 - 180 min | Average value: 64.2 min Grade Count:28 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |