Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 60 - 90 min | 60 - 90 min | Mass: 100g; TM R050-17 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Pot Life | 60 min | 60 min | |
NextGen Adhesives G907-32 Structural Adhesive Description: NGAC G907-32 is a thixotropic, epoxy adhesive system utilized extensively in staking, as well as, other industrial and structural applications.Advantages and Applications: The NGAC G907.. |
|||
Pot Life | 60 - 90 min | 60 - 90 min | Mass: 150g; TM R050-19 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Pot Life | >= 60 min | >= 60 min | |
Abatron 82098 A/B Filled Potting Compound
(discontinued **) Black "carbepoxll" abrasion resistant carbide filled epoxy. 100/12.5 ratio.Information provided by Abatron. |
|||
Pot Life | >= 60 min | >= 60 min | |
Abatron 85082 A/B Filled Potting Compound
(discontinued **) Black and colors casting, adhesive, potting, embedding, and coating system. 1/1 variable ratio.Information provided by Abatron. |
|||
Pot Life | 60 min @Temperature 25.0 °C |
60 min @Temperature 77.0 °F |
|
Lord Adhesives Thermosetâ„¢ MD-200 Electrically Conductive Die-Attach Adhesive This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured .. |
|||
Pot Life | 60 min | 60 min | |
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
Pot Life | 60 min | 60 min | 25 grams |
Tra-Con Tra-Bond 2143G Medium Viscosity Polyamide Epoxy Adhesive TRA-BOND 2143G is a medium viscosity adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This tw.. |
|||
Pot Life | 60 min | 60 min | 25 grams |
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive TRA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mixt.. |
|||
Pot Life | 60 min | 60 min | |
Tra-Con Tra-Bond FS279 Blush-Free Non-Sag Structural Epoxy Adhesive TRA-BOND FS-279 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This .. |
|||
Pot Life | 60 min | 60 min | |
Tra-Con Tra-Duct 916H04 Room Temperature Cure, Conductive Silver Epoxy Adhesive TRA-DUCT 916H04 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Pot Life | 60 - 90 min | 60 - 90 min | |
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs.. |
|||
Pot Life | 60 min | 60 min | 100 grams |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Pot Life | 60 min | 60 min | |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Pot Life | 60 min | 60 min | |
Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive A two-component, unfilled, flexible epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-109M-4 puts low stress on fragile parts a.. |
|||
Pot Life | 60 min | 60 min | |
Epoxyset Epoxibond EB-135 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-135 has excellent bond strength to various substrat.. |
|||
Pot Life | 60 min | 60 min | |
Epoxyset Epoxibond EB-301 Low Expansion Epoxy Adhesive EB-301 is a highly filled, low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional stability .. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | |
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and c.. |
|||
Pot Life | 60 min | 60 min | |
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond .. |
|||
Pot Life | <= 60 min | <= 60 min | |
ACC EP 2KSP EPI Engineered Polymers Silicone Modified Polyurea EP 2KSP Polyurea, “Powered by Reactamine® Technology”, is a 2 Component polyurea that reacts with aliphatic isocyanates to produce a high gloss, chemical resistant coating EP 2KSP can be used on .. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing. |
|||
Pot Life | 60 min | 60 min | 100 g |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Pot Life | 60 min | 60 min | |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Pot Life | 60 min @Temperature 25.0 °C |
60 min @Temperature 77.0 °F |
100 g |
Abatron AboCast 10-5/AboCure 3-4 Epoxy AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 3-4 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 3-4 is a tan room.. |
|||
Pot Life | 60 min | 60 min | Mass: 5g; TM R050-19 |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |
|||
Pot Life | 60 min | 60 min | |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |
|||
Pot Life | 60 - 90 min | 60 - 90 min | Mass: 50g; TM R050-19 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Pot Life | 60 - 90 min | 60 - 90 min | 100 gram batch |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |