Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 25.0 min @Temperature 23.9 °C |
25.0 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Pot Life | 25.0 min @Temperature 23.9 °C |
25.0 min @Temperature 75.0 °F |
|
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue Information provided by ITW Devcon |
|||
Pot Life | 25.0 - 30.0 min @Temperature 25.0 °C |
25.0 - 30.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2527 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 25.0 min | 25.0 min | uncured |
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr.. |