Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 1.00 min | 1.00 min | |
Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation This rigid polyurethane foam system is one of a family of polymer systems developed by Northstar Polymers for specific applications. Urethane foams molded with this system exhibit closed cell struct.. |
|||
Pot Life | 1.00 - 1.33 min | 1.00 - 1.33 min | |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |
|||
Pot Life | 1.00 min | 1.00 min | |
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Pot Life | 1.00 min | 1.00 min | |
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Pot Life | 1.00 - 105 min | 1.00 - 105 min | Average value: 23.8 min Grade Count:25 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |