Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 11 - 18 min | 11 - 18 min | Time before parts must be mated |
Lord Adhesives 7545D Two-Component, Equal-Mix, Non-Sag Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 15 - 18 min | 15 - 18 min | |
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works. |
|||
Pot Life | 15 - 18 min | 15 - 18 min | |
ITW Plexus Plexusâ„¢ MA330 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works.. |